MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco URSA® SAE 40 Premium TDX
Categories: Fluid; Lubricant

Material Notes: Texaco Ursa Premium TDX delivers value through:
  • Reduced wear — Prolonging component life and providing reduced maintenance costs.
  • Improved engine cleanliness — Providing efficient operation and reduced fuel consumption.
  • Extended drain capability — Reducing operating costs (approved by Mack, Cummins, Mercedes Benz, MTU, MAN).
  • Oil consumption control — Controls wear and piston deposits resulting in reduced emissions.
  • Engine durability even under arduous extended oil drain periods.

Texaco Ursa Premium TDX is a super high performance diesel engine oil (SHPD) specially designed for use in heavy duty turbocharged diesel engines with extended drain interval approval for various engine manufacturers.

Texaco Ursa Premium TDX, SAE 30 and 40, is recommended for four-stroke naturally aspirated, turbocharged, and supercharged diesel engines in all types of service.

It is ideal for mixed commercial fleets, farm machinery, construction equipment, marine and other off-highway applications.

It can also be used in four-stroke gasoline engines. Texaco Ursa Premium TDX, SAE 30 and 40, meets:

  • API Service Categories
    • CF, CD1
    • SL, SJ, SH, SG1
  • Major diesel engine manufacturers requirements
    • MTU/DDC Category 1
    • MAN M270
    • Mercedes Benz 228.1
    • Volvo VDS
  • Performance requirements of
    • Allison C4 Fluids (SAE 30)
    • Caterpillar TO-2 (SAE 30)
  • Manufacturers performance requirements
    • General Motors GM 6094-M
  • Department of Defense Commercial Item Description (CID)
    • A-A-52306A22

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Obsolete Specification.
  2. Engine performance equivalent to MIL-PRF-2104G, MIL-L-46152E.
  3. CPS Number: 222155; MSDS Number: 8603

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Ash, Sulfated Ash
  • Total Base Number, ASTM D2896
  • Pour Point
  • Flash Point
  • Phosphorus, P
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.