MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Shandong Rike Chemical HELI™ HL-531 PVC Foaming Regulator
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: The HL-series PVC foaming regulators acrylic processing aids and have all characteristics of acrylic processing aids. The only difference between them is that the molecular weight of foaming regulators is much more higher than that of processing aids.

Mechanism of Foaming Regulation

There are three purposes for filling the foaming regulators into PVC foaming products. The first one is to promote the fusion of PVC. The second one is to increase the melt strength of PVC so as to prevent from bubble amalgamation for obtaining even foaming products. The third one is to ensure perfect flow of melt for obtaining good appearance of the products. Owing to the difference of products, equipments for processing, raw materials and lubricant system, we developed several types of foaming regulators to satisfy the different requirements.

Information Provided by Shandong Rike Chemical Co., Ltd.

Vendors:
Available Properties
  • Bulk Density
  • Volatiles
  • Particle Mesh Size, <2%
  • Viscosity Measurement, intrinsic
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.