MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Graft Polymer GRAFTAMID™ EB-PA 01566 Ethylene Butyl Acrylate and Polyamide alloy
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: GRAFTAMID™ EB-PA 01566 is based on EBA matrix, and polyamide 66, with increased thermo-mechanical properties. Offers good barrier properties, chemical resistance, low moisture uptake and easy processing. Can be used as compatibilizer for PA blends/compounds or as a standalone material. Supplied as: Granulate.

Applications:

  • GRAFTAMID™ EB-PA 01566 has high service temperature
  • High melt temperature
  • Useful for cable compounds
  • Chemical packaging
  • PA blends and compounds.
Storage and Transportation: MSDS provided to recommend safe practices during usage. For easy handling and storage normally packed in 25 kg bags (50 bags per pallet).

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ISO 868
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527-2, Injection Molded. 20 mm/min.
  • Elongation at Break, ISO 527-2, Injection molded. 20mm/min.
  • Melting Point, DSC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Graft Polymer Ltd

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.