MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
VICTREX™ PEEK ESD101 Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: High performance thermoplastic with tight electrostatic dissipative control and low out gassing. ESD performance is not influenced by molding conditions provided that recommended processing conditions are rigorously controlled. Semi crystalline, granules for injection molding, easy flow, color black. Applications: semi-conductor industry where ESD control is essential while maintaining other performance requirements.

Information Provided by Victrex.

Vendors:
Available Properties
  • Density, ISO 1183, Crystalline
  • Viscosity, ISO 11443, Melt
  • Linear Mold Shrinkage, Flow, SO 294-4, 385°C nozzle, 180°C tool
  • Linear Mold Shrinkage, Transverse, SO 294-4, 385°C nozzle, 180°C tool
  • Spiral Flow, Victrex test, MoldTemp: 180°C, Melt Temp: 385°C
  • Outgassing - Total Mass Loss, ASTM E595, Water Vapor Regained
  • Outgassing - Total Mass Loss, ASTM E595
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527
  • Tensile Strength at Break, ISO 527
  • Tensile Strength at Break, ISO 527
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Unnotched (ISO), ISO 180/U
  • Volume Resistivity, IEC 60093, 100V
  • Surface Resistivity per Square, EOS/ESD S11.13, 100V
  • Surface Resistivity per Square, EOS/ESD S11.13, 10V
  • CTE, linear, Parallel to Flow, ISO 11359, below Tg
  • CTE, linear, Parallel to Flow, ISO 11359, above Tg
  • CTE, linear, Transverse to Flow, ISO 11359, below Tg
  • CTE, linear, Transverse to Flow, ISO 11359, above Tg
  • Thermal Conductivity, ISO 22007-4, Average
  • Thermal Conductivity, ISO 22007-4, Along flow
  • Melting Point, ISO 11357
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-f
  • Glass Transition Temp, Tg, ISO 11357, Onset
  • Glass Transition Temp, Tg, ISO 11357, Midpoint
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature, max 250°C
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.