MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Vinnolit® C 12/62 V Vinyl Chloride/Vinyl Acetate Copolymer Extender resin
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: Vinnolit® C 12/62 V Vinyl chloride/vinyl acetate copolymer extender resin for paste application. Vinnolit® C 12/62 V is a copolymeric extender resin having a high vinyl acetate content which has been specially developed for paste making. In blends with paste-making PVC resins, it combines the good viscosity-reducing properties of the homopolymer paste extender resins with the lower gelling temperatures typical of vinyl acetate copolymers. By incorporating an extender resin such as Vinnolit® C 12/62 V processing can be improved as the viscosity is considerably reduced, particularly in low plasticizer content and highly filled plastisols. By exchanging part of a copolymer paste resin the shelf life and deaeratibility are improved and dilatancy is reduced. The higher vinyl acetate content of Vinnolit® C 12/62 V allows lower gelling temperatures. The adhesion to various substrates, such as metal and synthetic fibers is improved. Vinnolit® C 12/62 V is particularly well suited for automotive underbody coatings and sealants, carpet backing and laminating pastes. Like all extender resins Vinnolit® C 12/62 V can be processed by all the standard methods, such as coating, dipping, casting and spraying.

Information provided by Vinnolit.

Vendors:
Available Properties
  • Volatiles, ISO 1269
  • Apparent Bulk Density, ISO 60
  • Particle Size, DIN EN ISO 53195, <= 0.5% Retained on 0.1 mm Sieve
  • Viscosity Test, ISO 1628-2, Reduced Viscosity
  • Vinyl Acetate Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.