MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Epoxies, Etc 10-3003 Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: 10-3003 is a new high bond strength epoxy adhesive formulated for ease in handling and convenience for the end user. This system has a non-critical mix ratio and adjustable flexibility. 10-3003 is also very safe to use due to the absence of harmful solvents and toxic chemicals in the formulation. 10-3003 yields high peel strength and excellent tensile strength. It also has outstanding thermal shock, impact and vibration resistance. This high performance epoxy adhesive exhibits outstanding physical, thermal, and electrical insulation properties. 10-3004 NC is available as a very low viscosity version of 10-3003. 10-3002 is available as a higher viscosity version of 10-3003.and polyol offer good low viscosity handling characteristics and turn thixotropic upon mixing.

Features:

  • Non-critical mix ratio
  • Excellent chemical resistance
  • Ability to adjust flexibility of bond line
  • Very good operating temperature range
  • Outstanding thermal shock resistance

Information provided by Epoxies, Etc

Vendors:
Available Properties
  • Specific Gravity, Catalyst
  • Specific Gravity, Resin
  • Viscosity, 10-3004NC Resin
  • Viscosity, 10-3002 Resin
  • Viscosity, 10-3002 Hardener
  • Viscosity, 10-3004 NC Mixed
  • Viscosity, 10-3003 Hardener
  • Viscosity, 10-3003 Resin
  • Viscosity, 10-3003 Mixed
  • Viscosity, 10-3004 Hardener
  • Viscosity, 10-3002 Mixed
  • Tensile Strength
  • Flexural Strength
  • Adhesive Bond Strength, PVC to PVC
  • Adhesive Bond Strength, Nylon to Nylon
  • Adhesive Bond Strength, Copper to Copper
  • Adhesive Bond Strength, Teflon*to Aluminum
  • Adhesive Bond Strength, Brass to Brass
  • Adhesive Bond Strength, Steel to Steel
  • Adhesive Bond Strength, Aluminum to Aluminum
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant, 10E3 cycles
  • Dielectric Strength
  • Dissipation Factor, 10E3 cycles
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Cure Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.