MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Chesterton 613 Moly Grease
Categories: Fluid; Lubricant

Material Notes: Description: Chesterton® 613 Moly Grease is a high-performance, cost-effective lubricant that can withstand extreme temperatures and pressures for a wide range of high and low-speed applications. Fortified with molybdenum disulfide, it can handle the toughest of lubricating jobs and last significantly longer than conventional greases. Wear, galling or seizing of greased surfaces can occur even when using high-performance greases, especially when heavy pressures squeeze the grease out of lubricating film. During these extreme pressure conditions, the molybdenum disulfide particles in 613 Moly Grease are left behind on the surface in a thin, adherent, lubricating film. The unique, plate-like geometry of the particles ensures that parts glide smoothly over each other, preventing wear, galling and eventual seizing. Until further applications of the grease can be applied. The product has excellent resistance to water washout, a condition that plagues and shortens the life of many conventional greases and necessitates constant re-lubrication. Since 613 Moly Grease ensures continuous, longer-lasting lubrication and protection, fewer applications are required. Less applications means less maintenance costs and less production downtime. The product’s superior mechanical stability assures that it will not break down or thin out and thus not leak out of the bearings under sustained heavy workloads.

Features:

  • Molybdenum disulfide for added boost under extreme conditions
  • Excellent mechanical stability
  • Corrosion inhibitors protect lubricated equipment
  • Excellent resistance to water washout
  • Special additives for longer life, continuous lubrication.

Benefits:

  • Reduce labor, maintenance costs
  • Reduce number of reapplications; low product costs
  • Save the cost of replacement parts
  • Prolong the life of machinery and parts

Applications: 613 Moly Grease lubricates all types of equipment in a wide range of applications that require a high-quality, long-lasting, cost-effective grease. It is especially effective on equipment subjected to extreme pressures during startup, shutdown or in operation. Use 613 Moly Grease for manufacturing and processing equipment

  • Conveyors
  • Mining equipment
  • Plain and anti-friction bearings
  • Small, exposed greats
  • Cams, guides, ways, slides
  • Press fittings and couplings
  • Electric motors
  • Fans, blowers
  • Pumps, generators
  • Presses, shears, hinges.

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Particle Size, Molybdenum disulfide
  • Four Ball Wear, 1800 rpm, 20 kg, scar diameter
  • Penetration, ASTM D217
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point, ASTM D566
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.