| Hostacom TRC 787N C4 NAT high melt flow mineral-filler filled thermoplastic elastomeric olefin(TEO) resin, has an excellent balance of processability, rigidity, and impact and scratch and mar resistance. It can be used for automotive interior applications, such as instrument panel, console, glove box. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Asia-Pacific Application: Automotive Parts; Instrument Panels; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Good Flow; Good Moldability; High Impact Resistance; Scratch Resistant Information provided by LyondellBasell. |