MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chesterton 752 Cold Galvanizing Compound
Categories: Fluid

Material Notes: Chesterton® 752 Cold Galvanizing Compound functions both as a zinc rich primer or final coating for ferrous metals and their welds exposed to atmospheric or corrosive conditions. The product deposits a 95% pure zinc coating that bonds to metal protecting it against corrosion both physically and by galvanic action. After fabrication or construction, it forms an all purpose protective coating. After wear, accidents, welding or maintenance work on galvanized protective coating. Chesterton 752 Cold Galvanizing Compound provides instant galvanizing. Unlike hot dip galvanizing, the product can be sprayed on to provide a convenient, fast drying protective coating.

Features:

  • 95% pure zinc in dried film
  • Ultra-fine particle size
  • Flexible
  • No heat required
  • Fast drying
  • Self healing
  • One part system
  • 3 way corrosion protection
  • Conforms to MIL-P-46105, MIL-P-21035 and MIL-P-26915
  • Authorized by the USDA

Applications: Use in maintenance and construction to restore damaged galvanized metal dn provide protection for all iron and steel surfaces, structures or equipment such as air conditioning units, agricultural machinery, automotive bodies, fences, marine equipment, metal floors and roofs, mining equipment and oil rigs, off shore drilling structures, ornamental iron works, pipe lines, railroad equipment, structural steel tanks, transmission towers, underground pipe lines, welds, ducts, marine equipment, decks etc.

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Impact Test, ASTM D2794, Extrusion
  • Impact Test, ASTM D2794, Intrusion
  • Maximum Service Temperature, Air
  • Processing Temperature, Application Temperature
  • Processing Temperature, Application Temperature
  • Dry Time, Touch
  • Dry Time, Recoat
  • USDA
  • Zinc, Zn, Dried Film
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.