MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Trinseo Magnum™ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 8391 MED ABS combines an excellent gloss appearance with high flow and medium impact performance. The mass (continuous process) ABS technology ensures an ABS resin that combines excellent processability with a stable light base color that is ideal for self-coloring. MAGNUM 8391 MED natural resin has undergone biocompatibility testing based on ISO 10993 (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications.

Applications:

  • Medical Applications

Information provided by Trinseo.

Vendors:
Available Properties
  • Density, ASTM D792
  • Apparent Bulk Density, ISO 60
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Melt Flow, ASTM D1238
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638, Injection Molded, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, Injection Molded, 50 mm/min
  • Tensile Strength, Yield, ISO 527-2/50, Injection Molded
  • Tensile Strength, Yield, ISO 527-2/100, Injection Molded
  • Tensile Modulus, ISO 527-2, Injection Molded
  • Flexural Strength, ASTM D790, 1.3 mm/min
  • Flexural Strength, ISO 178, Injection Molded, 2.0 mm/min, 3-points
  • Flexural Modulus, ISO 178, Injection Molded, 2.0 mm/min, 3-points
  • Flexural Modulus, ASTM D790, 1.3 mm/min
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180/A, Injection Molded
  • Izod Impact, Notched (ISO), ISO 180/A, Injection Molded
  • Charpy Impact, Notched, ISO 179/1eA, Injection Molded
  • Charpy Impact, Notched, ISO 179/1eA, Injection Molded
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Annealed
  • Vicat Softening Point, ISO 306/B50
  • Vicat Softening Point, ASTM D1525, Rate B (120°C/h), Loading 1 (10 N)
  • Flammability, UL94
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.