MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ISO-TECH ISO-LEN® 1000 PE-UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: ISO-LEN® 1000 has been proven for many years in various fields of application. Due to its wide range of characteristics, this all-round material is being used in products in all areas of technology where particularly high demands on material are required. By adding additives, we also deliver PE-UHMW finished parts with antistatic properties (ISO-LEN® 1000 AST) or with electrically conductive properties (ISO-LEN® 1000 EL).

Applications:

  • Beverage and packaging industries
  • Chemical and food industries
  • Mechanical and plant engineering
  • Electrical engineering and cryogenics
Types:
  • Sheet material (panels, cut-to-size, turned round bars)
  • Finished parts
Characteristics:
  • High abrasion resistance
  • Low friction coefficient
  • Self-lubricating
  • Very high notched impact strength

Information provided by ISO-TECH Kunststoff GmbH

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Water Absorption, ISO 62
  • Molecular Weight
  • Hardness, Shore D, ISO 868
  • Ball Indentation Hardness, ISO 2039-1
  • Tensile Strength, Yield, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Modulus of Elasticity, ISO 527-2
  • Charpy Impact, Notched, ISO 179
  • Coefficient of Friction, [µ]
  • Volume Resistivity, ISO 60093
  • Surface Resistance, ISO 60093
  • Dielectric Strength, IEC 60243
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Thermal Conductivity, DIN 52612
  • Melting Point, ISO 11357
  • Maximum Service Temperature, Air, long term
  • Maximum Service Temperature, Air, short term
  • Minimum Service Temperature, Air, short term
  • Minimum Service Temperature, Air, long term
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.