| (PBT+PC) GF30 FR(17), PBT+PC blend, 30% glass fiber reinforced, flame retardant (halogen based), low warpage Properties: dimensionally stable, good chemical resistance, Good electrical properties, good gliding properties, good fire behavior, High strength, High stiffness, High wear resistance, semi-crystalline Typical areas of application: Electronic components, Housing, Plug, Structural components, Connecting elements Industries: Automotive, Electrical and electronics industry, Household appliances, Mechanical Engineering, Sanitary industry Information provided by BARLOG plastics GmbH. |