MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco ISO 100 Utility Oil HVI
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Utility Oil HVI is a high quality, high viscosity index uncompounded oil with excellent water separating characteristics.

Chevron Utility Oil HVI possesses good natural thermal and oxidation stability.

Its high viscosity index makes it suitable for use over a wide temperature range.

In a circulating oil system, compressor, or lightly loaded gear case, it will maintain a high film strength, protecting metal parts.

Lubricant-related deposits will be kept to a minimum due to the excellent stability of this oil.

System contaminants such as dirt and moisture can be easily removed from this oil by proper filtration.

Chevron Utility Oil HVI ISO 68 is registered with NSF and is acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.

Applications

Chevron Utility Oil HVI is recommended:

  • for use in many circulating oil systems
  • • as a cylinder lubricant in double-acting reciprocating compressors
  • for the lubrication of both cylinders and running gears of single-acting compressors
  • for flushing lubricant systems, because of its compatibility
  • for hand oiling
Do not use Chevron Utility Oil HVI ISO 68 in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Key Words: CPS Number: 231213; MSDS Number: 6887
Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Pour Point, ASTM D97
  • Flammability Test, Fire Point °C
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.