MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Tra-Con Tra-Cast 3103 General Purpose Epoxy Casting Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST 3103 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating application where the combination of good mechanical thermal and electrical properties are required. It is an all liquid system with excellent flow and wetting characteristics, exhibits superior adhesion to glass, ceramics most metals, many plastics (includes potting shells) and other electronic materials, contains no solvents, and is easily mixed, handled and cured with minimum shrinkage at room temperatures. The fully cured TRA-CAST 3103 is an electrical insulator with good impact and thermal shock resistance. It is further resistant to water, weather, gases, galvanic action, petroleum fuels and solvents, alcohol, salts and many acids and alkalis.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Solids Content, Reactive Solids Content
  • Viscosity, After mixing
  • Hardness, Shore D
  • Adhesive Bond Strength, Lap shear, alum to alum, 2 hrs @ 65°C
  • Volume Resistivity
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, Ultimate Tg
  • Cure Time
  • Cure Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.