MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Mallard Creek Polymers Tykote® 1004 SBR Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: TYKOTE® 1004 is an anionic carboxylated styrene-butadiene copolymer latex. Features: exceptional water resistance, exceptional grease resistance, pigment compatible, very high tensile strength, flexible film properties, FDA approved for food contact. FDA Status: The ingredients of TYKOTE® 1004 comply with the FDA regulations listed below in 21 CFR governing components in food contact applications. 176.170 Components of Paper and Paperboard in Contact with Aqueous and Fatty Foods 176.180 Components of Paper and Paperboard in Contact with Dry Food. Storage and handling: protect from freezing. Ideal storage temperature is 22°C (72°F). Stability at 22°C (72°F) is 180 days when properly stored. Read the TYKOTE® 1004 Material Safety Data Sheet before handling, storing, or using this product.
APPLICATIONS: TYKOTE® 1004 is designed as a base resin for functional coatings. TYKOTE® 1004 provide high strength and pigment compatibility. This low surfactant containing copolymer can be used to compound functional coatings exhibiting superior water, water vapor, oil and grease repellency. TYKOTE® 1004 exhibits excellent mechanical stability and can be applied to a variety of substrates using many different application methods.

Information provided by Mallard Creek Polymers

Vendors:
Available Properties
  • Solids Content
  • pH
  • Brookfield Viscosity, #2/20 rpm
  • Glass Transition Temp, Tg
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.