MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ExxonMobil 120 Exxon Aviation Oil
Categories: Fluid; Lubricant

Material Notes: Aviation Oil 100, 120 and 20W-50 are  non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxidant, anti-foam and pour point depressant. Aviation Oil 100 and 120 are monogrades of SAE 50 and SAE 60 grade, correspondingly. Aviation Oil 20W-50 is a multi-grade lubricant. High manufacturing standards ensure the dependability of Aviation Oil under the exacting conditions of modern piston engine service. They are approved by leading engine manufacturers throughout the world.

Despite the advent and wide-spread use of ashless-dispersant aviation engine oils, some operators prefer to continue the use of non-dispersant mineral oil lubricants, which have provided excellent service for many years. In addition, many engine builders and overhaul agencies recommend or require the use of non-dispersant oils for break-in of new or newly overhauled engines. Aviation Oil of a viscosity grade selected to match the ambient temperature operation conditions of the aircraft meets these needs in accordance with the requirements of all major engine manufacturers. Aviation Oil products are U.S. Military approved under SAE J1966, which replaced MIL-L-6082E and are listed in the U.S. Military Qualified Products List QPL-1966. Specific viscosity grades are approved by Pratt and Whitney, Teledyne Continental Motors, and Textron Lycoming, and are included in their qualified products lists.

Vendors:
Available Properties
  • Density, ASTM D4052
  • API Gravity
  • Viscosity Measurement, ASTM D2270, Index
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Ash, SAE J1747
  • Total Acid Number, ASTM D664, mgKOH/g
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.