MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
BigRep HI-TEMP Biodegradable Polymer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: It is resistant to high temperatures, maintaining a constant resistance up to 160 °C with minimal warping. With such high heat resistance and an appealing matte surface finish, Hi-Temp filament is the choice for functional prototyping, household appliances, electrical casings, and as an end-use material for low-scale production or custom jigs and fixtures. Hi-Temp is a scale dynamic, allowing designs to maintain their quality between large-format and desktop 3D printers. Compatible with open printers like the BigRep ONE, Hi-Temp is an excellent ABS alternative that is easily printable in low-temperature environments. As a thermoplastic material derived from organic compounds, Hi-Temp is biodegradable under the correct conditions. CO2 neutral and environmentally friendly, it has a much lower ecological impact than other thermoplastics derived from fossil fuels - like ABS. Hi-Temp is FDA compliant for food safety and meets all requirements of EU Directives on food contact.

Highlights:

  • Heat Resistance up to 160 °C
  • Low Warping and Shrinkage
  • Environmentally Friendly Thermoplastic
  • Appealing Matte Finish
  • Food Safe

Information provided by Bigrep

Vendors:
Available Properties
  • Density, ISO 1183
  • Filament Diameter
  • Tensile Strength, ISO 527
  • Elongation at Break, ISO 527
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179-1 eU
  • Charpy Impact, Notched, ISO 179-1 eA
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Vicat Softening Point, ISO 306
  • Nozzle Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.