MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
TriStar TriSteel AC Metal Backed PTFE Bearing System
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricated environments. With lubrication, PV ratings can be met without limitations. Lubrication reservoirs are available on the liner to produce a constant storage and pumping action for better hydrodynamic film generation.

Vendors:
Available Properties
  • Density
  • Water Absorption
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Strength
  • Flexural Modulus
  • Compressive Strength
  • Compressive Strength, Maximum Static Bearing Load
  • Compressive Modulus
  • Coefficient of Friction, Dynamic, Dry vs Steel
  • K (wear) Factor
  • Limiting Pressure Velocity, Unlubricated. Max P = 36,000 psi and max V = 300 fpm
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Short Term
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
TriStar Plastics Corp.

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.