MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Bisalloy Steels Wear 500XT Steel, 8 - 25 mm
Categories: Metal; Ferrous Metal

Material Notes: BISALLOY® WEAR 500 XT is a 500 HB grade product with improved impact toughness developed recently at Bisalloy. It has excellent abrasion-resistance with guaranteed impact toughness, very good weldability and formability.

Applications: Being through hardened with a nominal hardness of 500 HB, BISALLOY® WEAR 500 XT has been developed for highly demanding applications and can offer an increased life expectancy in sliding and gouging abrasion situations. BISALLOY® Wear 500 XT is best suited to applications such as:

  • Dump Truck Wear Liners /Bodies
  • Mining Buckets
  • Cutting Edges
  • Chutes
  • Earthmoving Equipment
  • Underground Miners

Information provided by Bisalloy Steels Group Limited.

Vendors:
Available Properties
  • Hardness, Brinell
  • Tensile Strength
  • Tensile Strength, Yield
  • Charpy Impact, (Transverse)
  • Bend Radius, Minimum, Bend to 90 degrees, <16mm (Longitudinal)
  • Bend Radius, Minimum, Bend to 90 degrees, 16-25 mm (Longitudinal)
  • Bend Radius, Minimum, Bend to 90 degrees, <16mm (Transverse)
  • Bend Radius, Minimum, Bend to 90 degrees, 16-25 mm (Transverse)
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.