ForTii® C11-F is developed for low corrosion and has good balance in flow, toughness and stiffness, enabling thin walls or complicated geometries for E&E applications. C11-F has an all color V0 rating down 0.2mm and high RTI electrical rating of 140°C at 0.75 mm and a CTI of 800V to secure thermal ageing and electrical performance.