Hifax TYC 1235P B6A Rivian Black has a very high melt flow, very high flexural modulus, molded-in color, mineral-filled thermoplastic elastomeric olefin (TEO) resin that has an excellent balance of properties and processability. It is typically used for multiple automotive exterior trim applications. Availability: North America Application: Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Dimensional Stability; Good Impact Resistance; Good Moldability; High Flow; High Stiffness; Low Shrinkage Information provided by LyondellBasell. |