MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Wacker Belsil® DM 0.65 Disiloxane
Categories: Fluid; Polymer

Material Notes: BELSIL® DM 0.65 is a colorless, clear fluid of low viscosity and high volatility. It is non-polar and insoluble in water but miscible with alcohols, esters, and other solvents frequently utilized in cosmetics. Due to its low heat of vaporization, BELSIL® DM 0.65 evaporates from the skin without producing a cooling or stinging effect. BELSIL® DM 0.65 evaporates rapidly and without residues.

Application: BELSIL® DM 0.65 can be utilized as a delivery system in antiperspirant and deodorant formulations as well as hair-care products and color-cosmetic compositions. It helps to uniformly spread actives and pigments over the surface of hair and skin. It provides sufficient play time in color-cosmetics applications, thereby improving rub-in properties, reducing stickiness, and imparting lubricity and a smooth skin feel. In hair-care products BELSIL® DM 0.65 supports easy spreading of high-viscosity fluids, improves wet combability, and functions as a resin plasticizer in fixative styling products. To adjust drying times for specific product requirements, BELSIL® DM 0.65 may be blended in all proportions with other dimethicones and cyclomethicones.

INCI name: Disiloxane

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, DIN 51757
  • Kinematic Viscosity, DIN 53019
  • Surface Tension
  • Flash Point, DIN 51755
  • Ignition Temperature, DIN 51794
  • Refractive Index
  • Transmission, Visible, "Clear" but manufacturer does not quantify.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.