| CirculenRecover PPC TRC 228P NA Classic Black is a 12% talc filled polypropylene copolymer resin, with high impact resistance, very good flowability, good surface appearance and high UV resistance that contains recycled polypropylene resin. Product is available in pellet form. Status: Developmental Availability: North America Application: Exterior Trim Market: Automotive Processing Method: Injection Molding Attribute: Good Flow; Good Weather Resistance; High Impact Resistance; Pleasing Surface Appearance; UV Resistant Information provided by LyondellBasell. |