| Hostacom TRC 364N NAT is an 18% talc filled PP copolymer, with high flowability, good impact/stiffness balance, UV resistance and good scratch resistance. The product is available in natural color for self-coloring. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: High Flow; Scratch Resistant; UV Stabilized Information provided by LyondellBasell. |