MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik TROGAMID® CareMX97 Polyamide
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: TROGAMID® Care grades represent a range of both amorphous and microcrystalline transparent polyamides for processing via extrusion or injection molding. Durable: Microcrystalline TROGAMID® Care MX is the material of choice for all applications dealing with pharmaceutical formulations, lipids or aggressive disinfectants, since it exhibits an exceptional resistance towards chemicals and stress-cracking. Examples include fluid and drug delivery equipment such as stop-cocks, dialyzer parts, housings, covers or hearing aids. The high mechanical stability of amorphous TROGAMID® Care MT50 predestines the material for applications requiring a high modulus but retaining impact resistance which includes e.g. dentures, parts for monitoring and imaging devices or durable medical equipment. It comprises one of the highest tensile moduli compared to other transparent polyamides. Functional The antibacterial TROGAMID® Care MX73-A was designed to protect medical devices from surface bacterial colonization, while preserving its outstanding resistance to chemicals and stress-cracking as well as transparency. ISO 22196 tests conducted with E. coli and S. aureus showed a reduction of the viable cell count of more than 99.99%, each. TROGAMID® Care MX73-L is a transparent specialty grade for applications involving laser welding and laser marking. Though appearing transparent and colorless, it absorbs laser radiation, wherefore the combination of TROGAMID® Care MX73 and MX73-L enables the connection of two transparent parts via laser-welding, omitting exposure of the materials to extensive heat treatments or usage of adhesives. Target areas of application for TROGAMID® Care MX compounds include fluid and drug delivery systems, surgical instruments, housings, monitoring and imaging devices and durable medical equipment.

All advantages at a glance

  • High transparency
  • High chemical resistance
  • Very good stress crack resistance
  • UV resistance
  • High dynamic load-bearing capacity
  • Easy processability & colorability
  • Free of BPA

Information provided by Evonik

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527-1
  • Elongation at Break, ISO 527-1
  • Elongation at Yield, ISO 527-1
  • Tensile Modulus, ISO 527-1/-2
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Charpy Impact, Notched, ISO 179/1eA
  • CTE, linear, Parallel to Flow, ISO 11359
  • CTE, linear, Transverse to Flow, ISO 11359
  • Melting Point, ISO 11357
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306
  • Vicat Softening Point, ISO 306
  • Glass Transition Temp, Tg, ISO 11357
  • Flammability, UL94, IEC 60695
  • Flammability, UL94, IEC 60695
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.