MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman Spectar™ Renew 14471-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Spectar™ Renew 14471-50 copolyester is a sparkling, clear plastic material that is increasingly popular for protective barriers used to limit the spread of viruses like COVID-19, including sneeze guards. For these applications, Spectar™ Renew 14471-50 is a proven alternative to polycarbonate and acrylic. Eastman Spectar™ Renew 14471-50 copolyester is BPA free, environmentally friendly, fire and shatter resistant, long lasting, and resistant to common commercial cleaning agents. It can be found in a variety of end applications around the world, like point-of-purchase displays; separation barriers; signs; light fixtures at retailers, schools, hospitals, and office buildings; and sneeze guards. Facility managers prefer Spectar™ Renew copolyester for its excellent fire safety, chemical resistance, and versatility. It is the only clear plastic for heavy-gauge sheet applications that passes the National Fire Protection Association’s NFP 286 flammability test, required by many regional and national building codes. Unlike some materials, Spectar™ Renew 14471-50 is highly resistant to common cleaning agents, including many Spartan and Clorox products, enabling it to withstand discoloration and last longer. It is less brittle than acrylic polymers, allowing it to be easily shaped and formed to enable faster, easier installation. And best of all, surface scratches or scuff marks can be removed using a common heat gun. Retailers prefer Spectar™ Renew copolyester for point-of-purchase displays due to its aesthetically pleasing, crystal-clear, premium appeal that enhances the shopping experience. It is the material of choice for its glasslike appearance and ability to be shaped and curved. Sheet made from Eastman Spectar™ Renew copolyester is available throughout North America, Europe, Asia, and Latin America. Ask your contractor, fabricator, distributor, or e-retailer to specify Spectar™ Renew 14471-30 for your next project. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.GREENGUARD Certification recognizes Eastman for manufacturing products with low chemical and particle emissions for better indoor environments. For more information about GEI and to obtain printable certificates for Eastman copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the “Manufacturer” category and click search to display a list of our products. This product is certified to NSF/ANSI Standard 51 for Food Equipment Materials. This product has received a Platinum level Material Health Certificate from the Cradle to Cradle Products Innovation Institute. A Material Health Certificate is awarded to products that meet the Material Health requirements of the multi-attribute Cradle to Cradle Certified™ Product Standard. The Cradle to Cradle Products Innovation Institute is a nonprofit organization that administers the publicly available Cradle to Cradle Certified™ Product Standard, which provides designers and manufacturers with criteria and requirements for continually improving product materials and manufacturing processes. The Material Health Certificate provides manufacturers with a trusted way to communicate their efforts to identify and replace chemicals of concern in their products. For more information about Cradle to Cradle certification and to obtain printable certificates for Eastman copolyesters, visit www.c2ccertified.org. Search for Eastman Chemical Company in the Material Health Certificate Registry. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Building materials
  • Displays/in-store fixtures
  • Indoor signs
  • Lighting
  • Point-of-purchase
  • Shelving solutions-retail
  • Skylights
  • Thermoformed sheet
  • Visual merchandising
  • Walls
Key Attributes
  • Acrylic alternative (PMMA alternative)
  • BPA free
  • Easily formed and shaped
  • Free of materials of concern
  • Glasslike clarity
  • Naturally smooth edges
  • Passes NFP 286 flammability test
  • Polycarbonate alternative (PC alternative)
  • Popular for COVID-18 barriers and sneeze guards
  • Resilient to most commercial disinfectants and cleaning agents
  • Scratches can be easily removed with a common heat gun
  • Shatter resistant

Information provided by Eastman.

Vendors:
Available Properties
  • Density, ASTM D1505
  • Water Absorption, ISO 62, immersion
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ISO 527
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ISO 527
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ISO 527
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ISO 527
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Notched (ISO), ISO 180
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Puncture Energy, ASTM D3763, @ Max. Load
  • Puncture Energy, ISO 6603-2, @ Max. Load
  • Puncture Energy, ISO 6603-2, @ Max. Load
  • Puncture Energy, ISO 6603-2, @ Max. Load
  • Puncture Energy, ISO 6603-2, @ Max. Load
  • Puncture Energy, ISO 6603-2, @ Max. Load
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Short Time, 500 V/sec rate-of-rise
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • CTE, linear, ASTM D696
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Vicat Softening Point, ISO 306
  • Vicat Softening Point, ISO 306
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003
  • Gloss, ASTM D523, 60°
  • Yellow Index, ASTM D1925, CIELAB, Illuminant D6500, 10° Observer
  • Transmission, Visible, ASTM D1003, Regular
  • Transmission, Visible, ASTM D1003, Total
  • NSF Compliance, See notes for details
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.