MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Atom Adhesives AA-DUCT 903 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less than 3.8x10-2 ohm-cm. AA-DUCT 903 is recommended for electronic bonding and sealing applications that require both fine electrical and mechanical properties. AA-DUCT 903 has been used extensively in such diversified applications as microwave EMI & RFI shielding, in the assembly or repair of printed circuit boards, wave guides, electronic modules, flat cable, high frequency shields, connections, circuitry and as a cold solder for high-sensitive components where hot-soldering is impractical.

Appearance: Gray

Cure Type: Heat cure or Room Temperature

Benefits:

  • High strength
  • Perfect bond
  • Cold solder for high-sensitive components
Mix Ratio by weight: 100:5/Resin:Hardener

Substrates: Excellent choice aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.

Typical Application: Electrical, conductive, rmi/efi shielding, circuitry, printed circuit board and electronics repair

Information provided by Atom Adhesives

Vendors:
Available Properties
  • Specific Gravity, mixed, uncured
  • Solids Content, reactive, uncured
  • Linear Mold Shrinkage, cured
  • Hardness, Shore D, cured
  • Tensile Strength, cured
  • Compressive Strength, cured
  • Volume Resistivity, cured
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Heat Distortion Temperature
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Cure Time
  • Pot Life, uncured
  • Shelf Life, uncured
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.