MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Daikin DAIFREE GA-9700 Fluorocarbon Mold Release Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DAIFREE GA-9700 is an aerosol fluorocarbon mold release agent. It is solvent based and is combined with silicone. It shows enhanced performance in comparison to Daikin’s previous product, GA-7500. It also meets environmental regulations.

Introduction: High effective release performance with fluorocarbon as the principal ingredient; PFOA and PFOS free* and complies with environmental regulations such as TSCA and RoHS. *?5ppb detection limit; Little transfer, no stickiness left on the mold product; Minimal mold contamination is produced, reducing mold -cleaning requirements and improving productivity; A degassing cap is provided so that the aerosol product can be discarded safely

Information provided by Daikin.

Vendors:
Available Properties
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Daikin Industries

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.