MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Tropical Dark Red Meranti Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Variable, generally Moderately Durable (10 to 15 years) to durable
Resistance to penetration by preservatives: Resistant to extremely resistant
Common Applications: Interior and exterior joinery. Plywood

Key Words: Shorea spp.; Lumber, Timber
Vendors:
Available Properties
  • Specific Gravity, Green, Asian Origin
  • Density, Air Dry (12-15% Moisture Content)
  • Hardness, Wood Indentation, Side Hardness, Green, Asian Origin
  • Hardness, Wood Indentation, Side Hardness, 12% Moisture, Asian Origin
  • Modulus of Rupture, Static Bending, Green, Asian Origin
  • Modulus of Rupture, Static Bending, 12% Moisture, Asian Origin
  • Modulus of Rupture, Static Bending
  • Flexural Modulus, Static Bending, Green, Asian Origin
  • Flexural Modulus, Static Bending
  • Flexural Modulus, Static Bending, 12% Moisture, Asian Origin
  • Compressive Strength, Parallel to Grain, Green, Asian Origin
  • Compressive Strength, Parallel to Grain, 12% Moisture, Asian Origin
  • Compressive Strength
  • Machinability, Medium Relative to Other Wood
  • Shear Strength, Parallel to Grain, Green, Asian Origin
  • Shear Strength, Parallel to Grain, 12% Moisture, Asian Origin
  • Work to Maximum Load, Static Bending, Green, Asian Origin
  • Work to Maximum Load, Static Bending, 12% Moisture, Asian Origin
  • Shrinkage, Radial; Green to Zero Moisture
  • Shrinkage, Tangential; Green to Zero Moisture
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.