MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond Supreme 11HTLP One Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • High viscosity system
  • Convenient handling
  • Wide service temperature range
  • Thermal stability up to +400°F
  • Withstands thermal cycling
  • Superb adhesion to many substrates
Product Description: Master Bond Supreme 11HTLP is a high performance, higher viscosity, two part epoxy for bonding and sealing. It is exceptionally easy to use with a one to one mix ratio by weight or volume. Supreme 11HTLP has a convenient working life and cures readily at room temperature or more quickly at elevated temperatures. The optimum curing schedule is overnight at room temperature, followed by 2-3 hours at 150-200°F. Supreme 11HTLP is formulated to have imposing toughness, which in turn imparts high bond strengths in both the shear and peel mode. It also allows the system to resist demanding thermal cycling as well as impact and shock. Supreme 11HTLP bonds well to a wide variety of substrates, including metals, glass, ceramics, composites, many rubbers and plastics. It has good chemical resistance to water, oil and fuels. Upon curing, it is a dependable electrical insulator. Most significant is its very wide temperature range of -100°F to +400°F. Moreover, Supreme 11HTLP has low shrinkage upon curing, reliable dimensional stability and is readily machinable. The color of Part A is gray and Part B is amber. The very user friendly processing and top notch performance profile enables Supreme 11HTLP to be used in a wide variety of high-tech applications, especially in aerospace, electronics, specialty OEM and related industries.

Product Advantages:

  • Convenient mixing; non-critical one to one mix ratio by weight or volume
  • Easy to apply, higher viscosity system; good flow, favorable open time
  • Adheres well to a wide variety of substrates
  • Outstanding resistance to severe thermal cycling, impact and shock
  • Fine dimensional stability
  • Highly functional service temperature range

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B, thixotropic
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Strength
  • Adhesive Bond Strength, Tensile Lap, Aluminum to Aluminum
  • Peel Strength, aluminum to aluminum
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 gram batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.