MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Donnelly Bros APG #2 Super Clean All Purpose Mold Grease
Categories: Fluid; Lubricant; PTFE Gellant

Material Notes: Clear, non-melting PTFE (Teflon type) extreme pressure All Purpose Grease (APG). Odorless, with a Vaseline-like texture. 100% waterproof. Mineral oil base.

APG is used in the automotive, appliance, electrical and medical industries. APG is being used in injection molding presses, molds (guide pins-slides & ejector pins), grinders, electric motors and RIM (resists isocyanate).

Because APG #2 stays in place and and does not melt, it is beneficial in lubricating mechanical parts of molds. APG does not migrate works well in constant metal temperature of 180° F to 200° F. (Note: The plastic molding material itself might be 500-600° F.) APG contains PTFE, which plates the metal with a one micron film thickness which reduces friction. The acceptance rate of APG for this use is high.

APG is approved by Ford, GM, and Chrysler Toxicology Departments.

Information provided by Donnelly Bros. Inc.

Vendors:
Available Properties
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Donnelly Bros Inc

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.