| A bonded Tungsten Carbide facing for the toughest wear surfaces. Dyconite is an ultra-hard Tungsten Carbide Alloy that is diffusion-bonded to Steel or Iron substrates, employing space age technology. Advantages:- Provides greater wear and impact resistance than any other Overlay technology.
- Superior bond strength to low and high strength steels, abrasion resistant steels, stainless steels, cast irons and martensitic chromium white irons.
- Diffusion bond is stronger than steel.
- Good ductility allows material to bond to high hardness substrates or parts requiring hardening heat treatment without delaminating or cracking.
- Can be applied to existing or new parts
- Bendable to curved surfaces, internal contours and suitable to lining pipe.
- Saves on part wear and replacement as well as downtime and change-out time.
Applications: Mining: Dragline and dripper buckets, lip shroud bars, runners, ore chute liner plates, front end loader and grader blades wear plates, dredge points, centrifuge liners and plows, feeder chutes. Power Industry: Pulverizer hammers, pug mill paddles, inlet and exit coal fan blades, whizzer blades, cyclone liner plates, bull-nose wear plate Steel Industry: Flop gates, shot blast liners, side rails, impact element hammers Pulp and Paper: Debarker inserts and arms, chipper knives, chain and flight wear bars, grapple tine wear plates, pneumatic chip transition elbows, hog hammer tips, logging chain and flytes Glass and Grain: Cullet mixer paddles, grain mill hammersInformation from Wingate Alloys Inc. |