| KEBABLEND / H FE 220301/2 PET is a highly filled, soft magnetic PET compound with a density of 3.25 g/cm³ and is suitable as a metal substitute in low-load applications. Properties: dimensionally stable, High density, semi-crystalline, soft magnetic Industries: Automotive, Electrical and electronics industry, Household appliances, Mechanical Engineering Information provided by BARLOG plastics GmbH. |