MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Carpenter No. 484® (Carpenter Air-Hard; AISI A2)
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes: No. 484 tool steel is an air hardening steel capable of hardening throughout in heavy sections. It has been used for those applications in which the sections are very large and those involving extreme accuracy of size extreme hazards in hardening. It has a good balance between hardness and toughness. It is available as a DeCarb-Free product. DCF bars have been cold-finished in the mill therefore eliminating the need for bar bark removal.

Applications: Large blanking dies, Thread roller dies, Long punches, Rolls, Master hubs, Trimming dies, Forming dies, Precision tools, Gauges, Coining dies

Information provided by Carpenter Technology Corporation.

No. 484® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T30102
Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Rockwell C, Tempered at 1200°F
  • Hardness, Rockwell C, As hardened
  • Tensile Strength, Ultimate, when tempered at 400°F
  • Tensile Strength, Yield, when tempered at 400°F
  • Elongation at Break, when tempered at 400°F
  • Reduction of Area, when tempered at 400°F
  • Modulus of Elasticity
  • Izod Impact Unnotched, when tempered at 400°F
  • Abrasion, ASTM G65, loss in mm3, As-Hardened
  • Abrasion, ASTM G65, loss in mm3, Tempered at 1200°F
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Silicon, Si
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Carpenter Technology Corporation (Cartech)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.