MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chesterton 629 High Temperature White Grease
Categories: Fluid; Lubricant

Material Notes: Description: Superior resistance to washout by water, caustics, sanitizing cleaners, process fluids and steam has now been combined with high temperature performance to produce Chesterton 629 High Temperature White Grease. As a premium quality, water resistant grease, 629 will not be removed even in sever water washout situations. With a dropping point over 260°C, it will not melt and run out. 629 is NSF registered and complies with FDA regulations 178.3570 and 177.1550. It can be the exclusive lubricating grease used in food, beverage, meat, poultry and pharmaceutical plants. Chesterton 629 High Temperature White Grease is non-staining. Grease stains on floors, equipment, and packaging containers can be substantially reduced. Use 629 to lubricate textile machinery and paper converting equipment to virtually eliminate quality control rejects due to grease staining. Chesterton 629 is essentially tasteless and odorless. It is ideal as a maintenance or production lubricant used in food processing equipment, 629 contains no animal fats or oils which could become rancid.

Features:

  • Virtually impervious to water and steam
  • Dropping point over 260°C
  • PTFE Fortified
  • Smooth Tack Texture
  • Adheres to Metal
  • NSF H1 - Registration number 133936
  • FDA Compliant
  • Tasteless
  • Odorless

Suggested Uses: Use in all applications where conventional grease breaks down under shear, thermal abuse, or shock loading. Chesterton 629 High Temperature White Grease can be used wherever food-grade grease is required. Its functionality at higher temperatures and its translucent color provide added versatility.

Typical Applications:

  • Lubrication of slides, guides, plain bearings and bushings.
  • All types of anti-friction bearings
  • Grease-lubricated chains
  • Gears and cams
  • Joints and spline shafts
  • Other moving parts of equipment used in the manufacture of food, drugs and cosmetics such as: Bottle and carton filling machinery, Paste and sauce fillers, Conveyer belts and rollers, Fruit feeders and Canning machinery

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Kinematic Viscosity at 40°C (104°F), ASTM D445, Base Oil
  • Four Ball Extreme Pressure, Load Wear Index, ASTM D2596
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Penetration, ASTM D217
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point, ASTM D2265
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.