MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Plenco 1510 Polyester, Granular, Transfer Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester, Mineral Filled

Material Notes: PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file E40654. 01510 is available in black.

Information supplied by Plenco.

Vendors:
Available Properties
  • Bulk Density, ASTM D1895
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, ASTM D955
  • Hardness, Rockwell E, ASTM D785
  • Tensile Strength, Ultimate, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Poissons Ratio, ASTM D638
  • Shear Modulus, Calculated
  • Izod Impact, Notched, ASTM D256
  • Charpy Impact, Notched, ASTM D256
  • Impact, PLENCO, J/m Drop Ball Impact
  • Volume Resistivity, ASTM D247
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, Step by Step
  • Dielectric Strength, ASTM D149, Short Time
  • Dielectric Breakdown, ASTM D149, 1hr 120C
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, ASTM D3638
  • CTE, linear, ASTM E831, TMA
  • Thermal Conductivity, ASTM E1461
  • Maximum Service Temperature, Air, ASTM D570D, Heat Resistance
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Shrinkage, ASTM D1299, 72 hr, 120ºC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Plenco (Plastics Engineering Company)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.