MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Reynolds Sorta-Clear® 12 Silicone Rubber Compounds
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: SORTA-Clear™ Series rubbers are premium water white translucent silicone rubbers (platinum catalyst) which cure at room temperature with negligible shrinkage. Available in Shore 12A, 18A, 37A and 40A hardness, these rubbers feature high tensile and tear strength. SORTA-Clear™ 12 and SORTA-Clear™ 37 offer the convenience of a 1A:1B by volume mix ratio. The 18A and 40A products require a gram scale for measuring parts A + B. SORTA-Clear™ silicones are ideal for making prototype, jewelry or other molds of any configuration where model visibility is important (i.e. extracting a model from the mold via cutting). Materials such as urethane, epoxy or polyester resins can then be cast into SORTA-Clear™ silicone without application of a release agent. Other materials such as wax and low melt metal alloys can also be cast into SORTA-Clear™. SORTA-Clear™ can be pigmented with SILC Pig™ silicone pigments. SORTA-Clear™ 18, SORTA-Clear™ 37 and SORTA-Clear™ 40 are FOOD SAFE and can be used for culinary applications including casting chocolate and other confections. (See separate technical bulletin for usage instructions available at www.smooth-on.com). SORTA-Clear™ 12 is not food safe, and should not be used for food related applications. SORTA-Clear™ 18 is SKIN SAFE and certified by an independent laboratory.

Information provided by Reynolds Advanced Materials

Vendors:
Available Properties
  • Specific Gravity, ASTM D-1475
  • Viscosity, ASTM D-2393, Mixed
  • Linear Mold Shrinkage, ASTM D-2566
  • Hardness, Shore A, ASTM D-2240
  • Tensile Strength, ASTM D-412
  • Elongation at Break, ASTM D-412
  • 100% Modulus, ASTM D-412
  • Tear Strength, ASTM D-624, Die B
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Pot Life, ASTM D-2471
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.