MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 M320 Bearing Oil
Categories: Fluid; Lubricant

Material Notes: Bearing Oil M is a high-quality, rust and oxidation (R&O)-inhibited circulating oil specifically developed for the lubrication of backup roll bearings manufactured by Morgan Construction Company. It meets the performance requirements for “super demulsibility” as defined by Morgan’s Advanced Lubricant Specification, Revision 2.4, for use in hot and cold rolling mill operations. Bearing Oil M is formulated to provide rapid water separation, excellent oxidation resistance, protection against rust and corrosion, and resistance to foaming. It has excellent water-separating properties to minimize the formation of emulsions in circulating systems subject to contamination with large quantities of water, rolling solutions, dirt and scale. It has excellent oxidation resistance and thermal stability at high temperatures to minimize sludge and varnish formation, and provide long service life. It protects system components against rust and corrosion, and is resistant to excessive foam buildup that can interfere with proper lubrication.

Applications:

  • Backup roll bearings manufactured by Morgan Construction Company
  • Backup roll bearings in hot and cold rolling mills
  • Bearing lubrication in steel mills
  • Circulating systems where water contamination is a problem
  • Large, slow-speed gears in mixers and mills
Bearing Oil M meets the requirements of the following industry and OEM specifications:
  • Morgan Construction Advanced Lubricant Specification, Revision 2.4
  • U.S. Steel 135, Mill Circulating Oil
Features/Benefits:
  • Excellent water- separating properties
  • Excellent oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D2272, RPVOT
  • ASTM Color, ASTM D1500
  • Total Acid Number, ASTM D974, [mg KOH/g]
  • Pour Point
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.