MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell CirculenRecover C14 LD2420F LDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: CirculenRenew C14 LD2420 F is part of the Circulen© product family of circular and sustainable solutions. CirculenRenew C14 polymer reduces the carbon footprint as it replaces fossil feedstock through using renewable raw materials made from bio-based waste and residue oils. The renewable content of CirculenRenew C14 is measured by an accredited third party laboratory and stated as a parameter on the Certificate of Analysis (CoA). CirculenRenew C14 LD2420 F is a drop-in solution and therefore doesn’t require any adaptation of the existing processing equipment. CirculenRenew C14 LD2420 F is a non-additivated, low density polyethylene. It is characterized by a good melt strength leading to a good bubble stability during blown film extrusion. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications.

Status: Commercial - Active

Availability: Africa-Middle East; Asia-Pacific; Europe

Application: Agriculture Film; Bags & Pouches; Food Packaging Film; Hygiene Film; Liner Film; Shrink Film

Market: Flexible Packaging

Processing Method: Blown Film

Attribute: General Purpose; Good Heat Seal; Good Melt Strength; Good Optical Properties; Good Processability

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Melt Flow, ISO 1133-1
  • Tensile Strength, Yield, ISO 527-1, -2
  • Film Elongation at Break, MD, ISO 527-1, -3
  • Film Elongation at Break, TD, ISO 527-1, -3
  • Tensile Modulus, ISO 527-1, -2
  • Coefficient of Friction, ISO 8295
  • Dart Drop Test, ASTM D1709, F50
  • Film Tensile Strength at Break, MD, ISO 527-1, -3
  • Film Tensile Strength at Break, TD, ISO 527-1, -3
  • Melting Point, ISO 11357-3, Peak
  • Vicat Softening Point, ISO 306, A50
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 20°
  • Gloss, ASTM D2457, 60°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell LYB (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.