MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
SSAB Domex® 390XP Extra High-strength Cold-forming Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: Extra High-strength Cold-forming Steel, HSLA

Characteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of benefits compared to ordinary structural steels: Lower weight, Simpler production, Lower creep rate, Longer useful life, Higher load-bearing capacity, Lower transport costs, Reduced stocks, Lower overall cost.

Iron content is approximate - exact value is not reported by the manufacturer.

Data provided by SSAB Tunnplat.

Vendors:
Available Properties
  • Density, Estimated by MatWeb
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, A5
  • Bend Radius, Minimum, t<3mm; internal bend radius, 90°
  • Bend Radius, Minimum, 3 mm < t< 6mm; internal bend radius, 90°
  • Bend Radius, Minimum, t>6mm; internal bend radius, 90°
  • Iron, Fe
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.