MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
GEHR Plastics Ultem® PEI 1000
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance (operating temperature up to +338 °F), good dimensional stability and creep resistance. lts unique torque strength permits the economical substitution of machined fabricated small parts from steel.

Features: Very high strength and rigidity; High creep resistance; High torque strength and hardness; High thermostability; High weather resistance; High radiation resistance against ?-rays; Self-extinguishing; Limited resistance to stress cracks

Applications: Parts for electrical engineering; Parts for food industry; Parts for aircraft construction; Dosing stations; Fixings and spacers; Flanges and sleeves; Valves; Gear wheel

Information provided by GEHR Plastics, Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570, Humidity Absorption (saturation)
  • Water Absorption at Saturation, ASTM D570
  • Hardness, Rockwell R, ASTM D785
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dielectric Loss Index, ASTM D150
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Melting Point, ASTM D3418
  • Maximum Service Temperature, Air, UL746B
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ISO 306, VST/B/50
  • Minimum Service Temperature, Air, UL746B
  • Glass Transition Temp, Tg, ASTM D3418
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GEHR Plastics Inc

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.