MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Danquinsa DANTHANE® 126K-Powder TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: DANTHANE_ 126K-Powder is a polyester based, TPU-powder for transparent coatings. DANTHANE_ 126K-Powder is used for different powder sinter coatings. Furthermore this TPU is also suitable for laminations of different materials. It can also be used for thermoplastic adhesion equipments, for example for label material that will be applied later by thermobatch sealing process.

Application: DANTHANE_ 126K-Powder can be used at the coating as intermediate layer and final coating. This powder is best suitable for the lamination of textiles with supporting films by flat film lamination applications. This medium-hard TPU is mainly used for the coating of transport and conveyer belts as well as for flat belt material and flexible materials for containers. DANTHANE_ 126KPowder can also be combined with other DANADD_ powders in different colours. This can be used as intermediate layer and then as top coat DANTHANE_ 126K-Powder will be applied.

Information provided by Danquinsa GMBH

Vendors:
Available Properties
  • Density, DIN 53.479
  • Particle Size, Powder grit size
  • Melt Flow
  • Hardness, Shore A, DIN 53.505
  • Hardness, Shore D, DIN 53.505
  • Tensile Strength, DIN 53.504
  • Tensile Strength, DIN 53.504, Immersion in water
  • Elongation at Break, DIN 53.504
  • Elongation at Break, DIN 53.504, Immersion in water
  • Tensile Modulus, DIN 53.504
  • 100% Modulus, DIN 53.504
  • 300% Modulus, DIN 53.504
  • Resilience, DIN 53.512, [%]
  • Tear Strength, DIN 53.515, propagation resistance
  • Abrasion, DIN 53.516, [mm³]
  • Compression Set, DIN 53.517
  • Compression Set, DIN 53.517
  • Melting Point, Kofler
  • Softening Point, Kofler
  • Glass Transition Temp, Tg, DIN 51.007, DSC
  • Moisture Content
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.