MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals
Hafnium, Hf; Strip
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Tensile and/or hardness values are for Hafnium in strips; other property values are typical of the element. Three entries for pure Hf are in MatWeb.

Characteristics:

  • Contains approximately 250 ppm Dioxide which improves ductility
  • High Neutron absorption
  • Forms a stable, dense, self-healing oxide layer
  • High corrosion resistance
  • Allotropic transformation at 1760°C

Applications:

  • Superalloys
  • Alloying with Aluminium, Copper, Magnesium or Titanium
  • Nuclear systems - control rods

Vendors:
Available Properties
  • Density
  • Atomic Mass, 1995
  • Atomic Number
  • X-ray Absorption Edge, K
  • X-ray Absorption Edge, LI
  • X-ray Absorption Edge, LII
  • X-ray Absorption Edge, LIII
  • Electronegativity, Pauling
  • Ionic Radius, Crystal Ionic Radius for Valence +4
  • Tensile Strength, Ultimate, Longitudinal or Transverse
  • Tensile Strength, Ultimate, Transverse
  • Tensile Strength, Ultimate, Longitudinal
  • Tensile Strength, Yield, Longitudinal
  • Tensile Strength, Yield, Transverse
  • Tensile Strength, Yield, Longitudinal
  • Tensile Strength, Yield, Transverse
  • Elongation at Break, Longitudinal or Transverse, 50 mm
  • Elongation at Break, Longitudinal
  • Elongation at Break, Transverse
  • Electrical Resistivity
  • Magnetic Susceptibility, cgs/g
  • Critical Magnetic Field Strength, Oersted
  • Critical Superconducting Temperature
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Boiling Point
  • Hafnium, Hf
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.