| Product Information: Rubaloy - SS is a unique blend of Nitrile Rubber and Poly vinyl Chloride with a very high percentage of Plasticizers, etc. Test reports have proved that Rubaloy - SS has extremely good processing qualities. It has a unique low hardness quality with extremely good physical properties. Handling, cutting and weighing of Rubaloy - SS is easy as it comes in soft sheets, thus saving on time, cost and labor. Processing Characteristics: Rubaloy - SS can be easily processed on conventional Rubber mixing/compounding machines. It has excellent filler and plasticizer absorption properties and can withstand elevated, compounding temperatures. Applications: Since Rubaloy - SS has a very low polymer hardness not found in NBR / PVC blends. It has unique advantage to manufacture low hardness printing rollers, molded articles, low density foam, soft pipes, tubes and hoses. Information provided by Rubaloyâ„¢ |