| KEBATRON PPS L5530RC1 black is an impact modified, electrically conductive, 30% carbon fiber reinforced PPS compound, which is manufactured with post-industrial recycled carbon fibers. A large application potential lies in the substitution of metal housings (metal replacement/lightweight construction) with regard to EMC-compliant component design. As a housing material, KEBATRON PPS L5530RC1 black offers the advantage of electromagnetic shielding without additional surface treatments. Properties: antistatic, dimensionally stable, electrically conductive, good chemical resistance, good aging behavior, good fire behavior, high continuous used temperature, High strength, High stiffness, High wear resistance, semi-crystalline Typical areas of application: Valve caps, Distributor, Fasteners, Gears, Housing, Sliding elements, Plain bearing, Piston, Couplings, Bearing bushes, Pumps and motors, Pump housing, Sensors, Bobbin, Structural components, Transport chains, Valves Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Aviation Industry, Mechanical Engineering, Sports & Recreation Information provided by BARLOG plastics GmbH. |