MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
DSM Biomedical CarboSil® 5 Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyurethane, TP; Silicone Polyurethane, Polycarbonate Based

Material Notes: A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes

The silicone portion of CarboSil® TSPCU works synergistically with the polycarbonate component to improve stability. This medical grade polymer is highly biocompatible and well suited to be used in many types of medical devices.

Flexible CarboSil® TSPCU is comparable in tensile strength to traditional polycarbonate urethanes and derives additional biostability from the silicone portion. The material is adaptable to various fabrication techniques to accommodate many different device shapes. It can be extruded, injection or compression molded, solvent bonded, dipped coated and sprayed.

Widely Used Because of its tensile strength, biocompatibility and flexibility, CarboSil® TSPCU is used in a wide range of medical applications, including cardiovascular and nervous system electrostimulation, continuous glucose monitoring, drug eluting and orthopedic implants.

Tailor Made CarboSil® TSPCU can be enhanced with SME® technology to incorporate end groups that can address the needs of specific device applications (silicone end groups are standard). This eliminates the need for additional surface processing steps after the device component is fabricated.

Summary of Product Benefits

  • Biostable and biocompatible
  • Adaptable to many different processing techniques
  • Excellent mechanical properties
  • Thromboresistant
  • Enhanced with SME® technology
  • Comprehensive FDA Master File

Grade denotes silicone content (%)

Information provided by DSM Biomedical.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D1708
  • Tensile Stress at Strain, ASTM D1708
  • Tensile Stress at Strain, ASTM D1708
  • Tensile Stress at Strain, ASTM D1708
  • Elongation at Break, ASTM D1708
  • Processing Temperature, Optimum Extrusion Conditions
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DSM Biomedical (Former Polymer Technology Group)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.