MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ENrG Thin E-Strate® Zirconia Ribbon Ceramic Substrate
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Thin E-Strate® is flexible for economical patterning and moisture impermeable for longer product lifetimes. This flexible ceramic substrate offers a lower profile, lighter weight and increased durability. As this ceramic is inert, there is no concern for out gassing or impurities coming from the substrate. Surface roughness is 20 - 25nm and the material is easily coated by thick film, thin film and jetting processes. High temperature thin films can be deposited for higher quality and better performance. Used for thin film devices, portable electronics, solid state batteries, lightweight solar PV, durable labels, displays, sensors, protective cladding and bio-compatible devices.

Vendors:
Available Properties
  • Density, 99% Dense
  • Water Absorption
  • Water Vapor Transmission, 85% RH
  • Outgassing - Total Mass Loss
  • Hardness, Knoop, kg/mm²
  • Hardness, Mohs
  • Tensile Strength
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Strength
  • Poissons Ratio
  • Fracture Toughness
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Haze
  • IR Transmittance
  • Processing Temperature
  • Other, total
  • Y2O3, Mol%
  • ZrO2, Mol%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.