MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman G-3015 Maleic Anhydride Grafted Polypropylene
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Eastman™ G-3015 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites. Because of the polarity and anhydride functionality, Eastman™ G-3015 is useful for laminating, as a compatibilizer for PP blends with nylon or EVOH, and for enhancing the strength of composites that utilize reinforcements / fillers such as glass, talc, calcium carbonate, and metals. Eastman™ G series polymers are products of Eastman Chemical Company and are protected under one or more of the following U.S. patents: 5,955,547; 6,046,279; 7,408,007; 7,683,134; and their foreign equivalents.

Application/Uses:

  • Automotive
  • Building and Construction
  • Rubber and Plastic Modification
Key Attributes:
  • Balances attraction between polar fillers / reinforcements and non polar polymers
  • Coupling agent for PP composites
  • Maleic anhydride grafted polypropylene (PP)

Information provided by Eastman

Vendors:
Available Properties
  • Brookfield Viscosity, Solid at 125°C
  • Molecular Weight
  • Total Acid Number, [mg KOH/g]
  • Penetration, ASTM D5, [dmm], Needle under 100-g load for 5s @ 25 deg C, tenths of mm
  • Ring & Ball Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.