| Hifax TYC 1235X LS Black has a very high melt flow, very high flexural modulus, paintable, mineral filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of properties and processability. It is typically used for multiple automotive exterior applications. Availability: North America Application: Body Panels; Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Dimensional Stability; Good Impact Resistance; Good Moldability; High Flow; High Stiffness; Low Shrinkage; Paintable Information provided by LyondellBasell. |