  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Saint-Gobain MicaverĀ® Glass-Mica Electrical Insulator, Compression Moldings
Categories: Ceramic; Glass; Glass Ceramic; Machinable Ceramic

Material Notes: Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardness) typical of ceramics. It is made by mixing the components in powder form and heated under pressure. The glass particles melt and cover the mica flakes to form a hard, compact mass. It does not burn, is not hygroscopic, has high resistivity, is suitable for vacuum use, and has generally good chemical resistance - it is attacked by acetic, hydrochloric and nitric acid but resists sulfuric and phosphoric acids, ammonia, caustic soda, organic solvents, and saline solutions.

Applications include electric traction (railways, subways), busbar mountings, terminals, power cable mountings, switchbox mountings, and insulation of heating elements.

Information provided by Saint-Gobain Quartz PLC.

Vendors:
Available Properties
  • Density
  • Water Absorption
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Strength, Bending Strength
  • Compressive Strength
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint-Gobain Quartz PLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.